The surface of steel after laser cutting is ready for enduse.

This part illustrates well the quality after laser cutting. When cutting 15mm thick steel with 5kW Trumpf Trulaser machine the surface is ready for enduse.
The cutting speed is 1500mm / 6 min. Before surface treatment an oxidfilm removal is recommended, the result can be seen on the photo and the film.  
One of the part is before, the other one is after the removal. For mechanical engineering and structure construction this is a perfect quality!

Lasercut surface before and after oxidfilm removal     Lézervágott normál acél oxidfilm eltávolítás előtt és után

 

Melior Laser Ltd. H-2051 Biatorbágy, Tormásrét u. 5/B.
Phone: +36 23 313 270     info@meliorlaser.hu
Copyright © 2024 Sheet metal fabrication, sheet metal part production, powder coating in Hungary - Melior Laser Ltd.
All rights reserved.
Designed by One Online

EU funds

  • Last Modified: Thursday 28 March 2024, 13:27:21.